ASTM D6095 Standard Test Method for Longitudinal Measurement of Volume Resistivity for Extruded Crosslinked and Thermoplastic Semiconducting Conductor and Insulation Shielding Materials

Zoom  Zoom Issue Date:2012-02-08   Browse:894
ASTM D6095挤制交联和热塑半导性导体和绝缘防护材料体电阻率的经度测量标准试验方法
ASTM D6095 Standard Test Method for Longitudinal Measurement of Volume Resistivity for Extruded Crosslinked and Thermoplastic Semiconducting Conductor and Insulation Shielding Materials
ASTM D6095挤制交联和热塑半导性导体和绝缘防护材料体电阻率的经度测量标准试验方法

The electrical behavior of semiconducting extruded shielding materials is important for a variety of reasons, such as safety, static charges, and current transmission. This test method is useful in predicting the behavior of such semiconducting compounds. Also see Test Method D 4496.
1. Scope
1.1 This test method covers the procedure for determining the volume resistivity, measured longitudinally, of extruded crosslinked and thermoplastic semiconducting, conductor and insulation shields for wire and cable.
1.2 Whenever two sets of values are presented, in different units, the values in the first set are the standard, while those in parentheses are for information only.
This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. For a specific hazard statement, see .
1.3 In common practice the conductor shield is often referred to as the strand shield.
1.4 Technically, this test method is the measurement of a resistance between two electrodes on a single surface and modifying that value using dimensions of the specimen geometry to calculate a resistivity. However, the geometry of the specimen is such as to support the assumption of a current path primarily throughout the volume of the material between the electrodes, thus justifying the use of the term "longitudinal volume resistivity." ( See 3.1.2.1 )

2. Referenced Documents (purchase separately)
ASTM Standards
D257 Test Methods for DC Resistance or Conductance of Insulating Materials
D1711 Terminology Relating to Electrical Insulation
D4496 Test Method for D-C Resistance or Conductance of Moderately Conductive Materials
Index Terms
conductor shield; conductor shielding material; insulation shield; insulation shielding material; moderately conductive; semiconducting shielding materials; semiconducting shields; volume resistivity of shielding materials;
 
 
[ Fire test center Search ]  [ ]  [ Forword to friends ]  [ Print ]  [ Close ]  [ Back to Top ]

 

 
 
Home | About us | Contact | Terms & Conditions | Copyright | Site Map | Friend link | Guestbook | Old Version | 闽ICP备09009213号
©2013-2015 FIRETC.NET All Rights Reserved   ICP:闽ICP备09009213号-4